Product Details:
Payment & Shipping Terms:
|
Tank Steel Shell: | 5mm, 6mm | Lining: | LDPE 16mm |
---|---|---|---|
Compartment: | 1,2,3,4 | Good For Hazardous Cargoes: | Ammonia Liquid, Glacial Acetic Acid, Dilute Sulfuric Acid, Hydrochloric Acid,Caustic Soda |
Certificate Of Origin: | China CO /Favour/ACFTA/ Form E | Import Tax: | 0% |
HS-Code: | 8707909000 | Cell: | 8615271357675 |
High Light: | van truck bodies,steel truck bodies |
Chemical Tank For Hcl Cargo Hydrochloric Acid Tank Body 17500Litres Steel Lined PE 16mm -18mm
steel lined PE 16mm -18mm LDPE
Shell 5mm, 6mm
Tank net Capacity: 11000L ~12000L
3compartments
good for the SODIUM HYPOCHLORITE transport.
good for the HYDROCHLORIC ACID transport
Acid tank truck body 3~36m3 truck body Customization, Cost Control Built How You Want it, at a Price You Can Afford.
Description of goods | Quantity | Unit price (USD) | Amount (USD) |
Over all size: 6100*2200*2200m3 Steel sheet 6mm Three compartments Liner thickness: 16mmPE Detail as draw No.: JDT-0109-159 agreed by both size
|
02pc | 12,300 | 24,600 |
Capacity: 22m3 Steel sheet 6mm Liner thickness: 16mmPE Tank in rectangular frame Detail as draw agreed by both size |
04pc | 12,300 | 49,200 |
Price Term : FOB SHANGHAI
+ Port of loading : Shanghai Port
+ Port of unloading : Hochiminh Port.
Description of goods | Quantity | Unit price (USD) | Amount (USD) |
Chemical Tank For Hcl Cargo Truck Tank Size :5100*2350*1400mm Over all size 5100*2350*1820mm Steel sheet 6mm Three compartments Liner thickness: 16mmPE Detail as draw agreed by both size |
06Units |
FOB$12,300
|
FOB$73,800 |
Total in USD | FOB$73,800 | ||
Say: Seventy three thousand eight hundred US dollars only
SHIPMENT: Shipped on board within 50 days from date of 50% downpayment + Partial shipment : allowed + Port of loading : Any China Port + Port of unloading : HCMC Port/ Cat Lai port |
send following documents to Buyer:
for sale call:+86-152 -7135-7675
+ Port of loading : Shanghai Port + Port of unloading :buenos aires port Country of Destination: Argentina |
Description of goods | Quantity | Unit price | Amount | |
Chemical liquid tank for truck steel lined PE 16mm Shell 6mm Tank net Capacity: 15000L 3 compartment of 5000 lts |
1 | $13,000 | $13,000 | |
Chemical liquid tank for truck steel lined PE 16mm Shell 6mm Tank net Capacity: 25500L3 compartment of 8500 lts |
3 | $18,000 | $54,000 | |
FREIGHT AND INSURANCE COST TO | $2000-$3000/40HQ | $0 | ||
CIF$67,000buenos aires port | ||||
Say: US dollars only.. | ||||
VA lid in 20days Delivery time: 35 days after receipt of 50% deposit, 25 days 100% deposit; |
||||
Packing: WAXED for sea transport | ||||
Terms of payment: By T/T ;50%downpayment ,50% pre-shipment |
CBU terms should be chosen for such tanker shipment.
DRZ tank is specially design for the (storage /transporting) transportation bleach, hydrochloric acid, ferric chloride, oilfield chemicals, corrosive wastes and other hazardous cargoes. The tank size is Customization,normally 3-30 cubic meter, the basement/beam of tanker have locks which enable the tanker to be fixed on a standard chasiss or trailer. The tanker body adopts steel plate optional, 5/6mm in thickness with 2~4 compartments. The discharging is normally by gravity. Pumps can be used as an option. Other facilities provided included manholes, lipsticks, discharging valves, ladders. The tanker body will be painted with logo or any banners that the customer assigns.
We make the Acid tank Truck Parts
Acid tank truck body truck body from 3 to 36 CBM capacity, we can make with the capacity as your request. Good design for long using life.
Basic Chemicals Tanks for reactor/ storage or transport
Caustic Soda (NaOH) Tanks
Sulphuric Acid (H2SO4) Tanks
Hydrochloric Acid (HCl) Tanks
Phosphoric Acid (H3PO4) Tanks
Liquid Ammonia (NH3) Tanks
Javel (NaOCl) Sodium hypochlorite Tanks Ect.
LDPE & HDPE polyethylene resistance listed by chemical
1.4-dioxane LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
some effect after 7 days of constant exposure.
Acetaldehyde LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE at 50C° shows
some effect after 7 days of constant exposure. LDPE - immediate damage may occur.
Acetic Acid 5 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Acetic Acid, glacial 50% LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50 C° -
immediate damage may occur.
Acetone LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Allyl Alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Aluminum salts LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Amino acids LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonia LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium carbonate,
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium phosphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium sulphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Amyl chloride HDPE at 20C° shows some effect after 7 days of constant exposure. HDPE at 50C° and LDPE at 20C°-50C° -
immediate damage may occur. Not recommended for continuous use.
Aniline LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE at 50C° shows
some effect after 7 days of constant exposure.
Benzene LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Benzyl alcohol LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Boric acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Bromine LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Butyric acid LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Calcium chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Calcium hydroxide
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Calcium sulphate No data is available at this time.
Carbon tetrachloride HDPE at 20C° shows little or no damage after 30 days. LDPE at 20C° and HDPE at 50C° show some effect
after 7 days of constant exposure. LDPE at 50C° not recommended.
Chlorobenzene Immediate damage may occur. Not recommended for continuous use.
Chloroform HDPE and LDPE at 20C° show some effect after 7 days. At -50C° - immediate damage may occur. Not
recommended for continuous use.
Chlorine 10% in water HDPE and LDPE at 20C° shows little or no damage after 30 days. LDPE at 50C° shows damage and is not
recommended.
Chromic acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Chromic acid 50% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Citric acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Cresol HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° show immediate
damage and are not recommended for continuous use.
Cyclohexane LDPE and HDPE at 50C° - immediate damage may occur. HDPE and LDPE at 20C° show some effect after 7
days of constant exposure.
Diethyl ketone LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Dimethylsulfoxide LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethanol 95% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. Ethyl acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethyl benzene HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° show immediate
damage and are not recommended for continuous use.
Ethylene glycol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethylene oxide HDPE at 20C° shows little or no damage after 30 days of constant exposure. LDPE at 20C° and LDPE/ HDPE
at 50C° show some effect after 7 days.
Ferric chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Fluoride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Fluorine HDPE at 20C° shows little or no damage after 30 days of constant exposure. LDPE at 20C° shows some effect
after 7 days. Neither HDPE or LDPE are recommended at 50C°.
Formaldehyde 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Formaldehyde 40% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Glycerol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Heating oil No further data is available at this time.
Hexane HDPE at 20C° shows little or no damage after 30 days continuous use and at 50 C° shows some effect after 7
days. LDPE not recommended at any temperature.
Hydrochloric acid 5% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrochloric acid 20% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrochloric acid 35% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrocyanic acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid 4% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid 48% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrogen peroxide 3% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrogen peroxide 30% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Isobutyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Isopropyl acetate No data is available at this time.
Isopropyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Kerosene LDPE and HDPE at 20C° show some effect after 7 days. HDPE and LDPE not recommended at 50C°, as
immediate damage may occur.
Lactic Acid 10 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Lactic Acid 90 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Lead acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Metallic salts, dissolved No data is available at this time.
Methanoic acid 100% No data is available at this time.
Methanol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Methyl ethyl ketone Immediate damage may occur. Not recommended for continuous use.
Methyl propyl ketone HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° - Immediate damage
may occur. Not recommended for continuous use.
Methylene chloride HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° - Immediate damage
may occur. Not recommended for continuous use.
Mineral oil LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° may
show immediate damage and is not recommended.
n-amyl acetate LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
some effect after 7 days or constant exposure.
n-butyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
n-octane LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Nitric acid 50 % LDPE at 20C° shows little or damage after 30 days. HDPE at 20C° and LDPE at 50C° show effect after 7 days.
HDPE at 50C° shows immediate damage and is not recommended.
Nitric acid 70 % HDPE and LDPE at 20C° show some effect after 7 days. Both at 50C° show immediate damage and are not
recommended.
Oleic acid HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. LDPE at 20C°-50C° shows
immediate damage and is not recommended.
Oxalic acid LDPE at 20C° shows some effect after 7 days. HDPE at 20C° and both HDPE and LDPE at 50C° show little or
no damage after 30 days.
Ozone HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE and LDPE at
50C° show immediate damage and are not recommended.
Perchloric acid HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE and LDPE at 50C° show immediate damage and are not recommended.
Perchloric ethylene HDPE and LDPE at 20C°-50C° show immediate damage and are not recommended.
Phenol HDPE and LDPE at 20C°-50C° show immediate damage and are not recommended.
Phosphoric acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Phosphoric acid 85% HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
immediate damage and is not recommended.
Phosphorous trichloride HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° has no
data available. HDPE at 50C° shows some effect after 7 days.
Potassium acetate No data is available at this time.
Potassium bromide No data is available at this time.
Potassium carbonate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium hydroxide 5 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium hydroxide
concentrated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium permanganate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Propylene glycol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Pyridine Immediate damage may occur. Not recommended for continuous use.
Salicylic acid, saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Silver acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Silver nitrate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium carbonate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium chloride,
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium dichromate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium hydroxide 1% LDPE at 20C°-50C° shows little or no damage after 30 days of constant exposure. HDPE at 20C°-50C° shows
some effect after 7 days.
Sodium hydroxide 50% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium hypochlorite 15% HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. LDPE at 20C° is suitable but
at 50C° shows some effect after 7 days.
Sodium nitrate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium sulphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sucrose LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulphide No additional information is available at this time.
Sulfuric acid 6% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 20% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 60% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 98% LDPE at 20C°-50C° shows little or no damage after 30 days of constant exposure. HDPE at 20C° shoes effect
after 7 days and is not recommended for use at 50C°.
Tannic acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Tetrahydrofuran HDPE and LDPE at 20C° show some effect after 7 day of constant exposure.HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Toluene LDPE at 20C° show some effect after 7 day of constant exposure. HDPE at 20C°-50C° and LDPE at 50C°
show immediate damage and are not recommended.
Trichloracetic acid HDPE and LDPE at 20C° show some effect after 7 day of constant exposure.HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Trichlorethane Immediate damage may occur. Not recommended for continuous use.
Turpentine oil HDPE and LDPE at 20C° show some effect after 7 day of constant exposure. HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Urea LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Xylene HDPE at 20C° shows some effect after 7 day of constant exposure. LDPE at 20-50C° and HDPE at 50C° show
immediate damage and are not recommended.
Zinc chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.