Product Details:
Payment & Shipping Terms:
|
Tank Steel Shell: | 6mm, 8mm | Baffles: | 6,8 |
---|---|---|---|
Good For Hazardous Cargoes: | H2SO4 98% Concentrated Sulfuric Acid | Certificate Of Origin: | China CO /Favour/ACFTA/ Form E |
HS-Code: | 8707909000 | Cell: | 8615271357675 |
Tri-axle: | FUWA,L1.BPW | Suspension: | Spring OR Aire Bag |
High Light: | chemical road tankers,chemical tank trailers |
Sulphuric Acid Tanker Trailer V shape 18500L,19000L,21000L for Zambia
steel Shell 6mm, 8mm
Tank net Capacity: 17000L ~21000L
Description of goods | Quantity | Unit price | Amount | Description of goods | |
tri axle Acid tanker V SHAPE Half chassis |
tri axle Acid tanker BPW spring suspension, 12R22.5 tire, Tank net Capacity:21,000ltres to carry acid with SG 1.83,shell of tank 6mm carbon steel add Strengthen rolled steel rings reinforcement, end of the tankers with 8mm carbon steel V SHAPE Half chassis |
10units |
FOB$19800 |
FOB$198000.00 | |
Freight cost : | Shipping line for the shipment | ||||
TOTAL | Saying: USD dollars only. | ||||
CIF73200USDShip to Dar es Salaam port |
Customization, Cost Control Built How You Want it, at a Price You Can Afford.
for sale call:+86-152 -7135-7675
Specification 21,000 liter Acid tanker Semi trailer specifications just for reference
DIMENSIONS | |
Tare Weight | 9090kg( VIN plate can write 7500KG) |
Payload | 32000-38400 kg(32500kg) |
Total Weight | 41090-47490kg(40000kg) |
Overall Length | 12000mm |
Overall Width | 2500mm |
Overall Height | 3500mm |
Wheel track | 2050/2050/2050 Refer drawing mm |
Wheel base | 5790+1360+1360 Refer drawing mm |
STANDARD SPECIFICATION | |
Main Frame | Heavy duty and extra durability designed; Opting for high tensile steel Q345B, Middle Flange 6mm ;Bottom Flange 10mm,width 100mm- 140mm |
Axle | Three fuwa axles. Or L1 axles, BPW axles optional add $1000 |
Suspension |
3 BPW axle spring Suspension airbag suspension add$6600 FUWA airbag suspension optional add$3640 |
Landing Gear | Two-speed ,manual operation, heavy duty landing gear |
Wheel Rim | Twelve units of 9.0wide x 10 stud (tubeless rim) |
Tyre |
12 units of 12R-22.5 tyres (tubeless) or 6 units of 385/65R22.5 super single tires |
Spare Wheel Carrier | two spare wheel carrier including a riser |
Pneumatic Braking System | 30/30 spring brake chamber (S Cam); eliable local brand 40L air tank ; reliable local brand standard coppery air-connector. With ABS axle |
Electrical System | 24V 7-pin socket; reliable local brand standard red rear lights, orange turning lights, red rear reflectors, 3 orange side lights and 3 orange side reflectors each side 6, standard Cable. |
Tank | 21,000 litres capacity for H2SO4 98% |
shell of tank 6mm /baffles 5mm carbon steel add Strengthen rolled steel rings reinforcement, end of the tankers with 8mm carbon steel | |
Walkway and top tank; stainless steel ladder end or side of tank | |
Tank fittings |
Manhole covers top filler and spillbox, Bottom coupling two valves : one SS316 ball DN80, one PTFE lined butterfly valve discharge system : stainless steel pipes |
Tool box | One tool box,one water tank, one lime box |
Painting | Sand blasting before painting; two coats of primer, anti corrosion, two coats of finish painting; (black chassis, blue tank or as client requirement) |
CBU terms should be chosen for such tanker shipme
DRZ tank is specially design for the transportation hazardous cargoes Sulphuric .
The discharging is normally by gravity. Pumps can be used as an option. Other facilities provided included manholes, lipsticks, discharging valves, ladders. The tanker body will be painted with logo or any banners that the customer assigns.
Cell: 0086 152 7 135 7635 ; 0086 152 7 135 7675
WhatsApp: 8615271357675 tictrucks#gmail.com
LDPE & HDPE polyethylene resistance listed by chemical
1.4-dioxane LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
some effect after 7 days of constant exposure.
Acetaldehyde LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE at 50C° shows
some effect after 7 days of constant exposure. LDPE - immediate damage may occur.
Acetic Acid 5 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Acetic Acid, glacial 50% LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50 C° -
immediate damage may occur.
Acetone LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Allyl Alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Aluminum salts LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Amino acids LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonia LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium carbonate,
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium phosphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium sulphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Amyl chloride HDPE at 20C° shows some effect after 7 days of constant exposure. HDPE at 50C° and LDPE at 20C°-50C° -
immediate damage may occur. Not recommended for continuous use.
Aniline LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE at 50C° shows
some effect after 7 days of constant exposure.
Benzene LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Benzyl alcohol LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Boric acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Bromine LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Butyric acid LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Calcium chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Calcium hydroxide
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Calcium sulphate No data is available at this time.
Carbon tetrachloride HDPE at 20C° shows little or no damage after 30 days. LDPE at 20C° and HDPE at 50C° show some effect
after 7 days of constant exposure. LDPE at 50C° not recommended.
Chlorobenzene Immediate damage may occur. Not recommended for continuous use.
Chloroform HDPE and LDPE at 20C° show some effect after 7 days. At -50C° - immediate damage may occur. Not
recommended for continuous use.
Chlorine 10% in water HDPE and LDPE at 20C° shows little or no damage after 30 days. LDPE at 50C° shows damage and is not
recommended.
Chromic acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Chromic acid 50% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Citric acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Cresol HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° show immediate
damage and are not recommended for continuous use.
Cyclohexane LDPE and HDPE at 50C° - immediate damage may occur. HDPE and LDPE at 20C° show some effect after 7
days of constant exposure.
Diethyl ketone LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Dimethylsulfoxide LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethanol 95% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. Ethyl acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethyl benzene HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° show immediate
damage and are not recommended for continuous use.
Ethylene glycol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethylene oxide HDPE at 20C° shows little or no damage after 30 days of constant exposure. LDPE at 20C° and LDPE/ HDPE
at 50C° show some effect after 7 days.
Ferric chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Fluoride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Fluorine HDPE at 20C° shows little or no damage after 30 days of constant exposure. LDPE at 20C° shows some effect
after 7 days. Neither HDPE or LDPE are recommended at 50C°.
Formaldehyde 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Formaldehyde 40% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Glycerol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Heating oil No further data is available at this time.
Hexane HDPE at 20C° shows little or no damage after 30 days continuous use and at 50 C° shows some effect after 7
days. LDPE not recommended at any temperature.
Hydrochloric acid 5% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrochloric acid 20% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrochloric acid 35% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrocyanic acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid 4% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid 48% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrogen peroxide 3% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrogen peroxide 30% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Isobutyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Isopropyl acetate No data is available at this time.
Isopropyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Kerosene LDPE and HDPE at 20C° show some effect after 7 days. HDPE and LDPE not recommended at 50C°, as
immediate damage may occur.
Lactic Acid 10 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Lactic Acid 90 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Lead acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Metallic salts, dissolved No data is available at this time.
Methanoic acid 100% No data is available at this time.
Methanol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Methyl ethyl ketone Immediate damage may occur. Not recommended for continuous use.
Methyl propyl ketone HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° - Immediate damage
may occur. Not recommended for continuous use.
Methylene chloride HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° - Immediate damage
may occur. Not recommended for continuous use.
Mineral oil LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° may
show immediate damage and is not recommended.
n-amyl acetate LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
some effect after 7 days or constant exposure.
n-butyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
n-octane LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Nitric acid 50 % LDPE at 20C° shows little or damage after 30 days. HDPE at 20C° and LDPE at 50C° show effect after 7 days.
HDPE at 50C° shows immediate damage and is not recommended.
Nitric acid 70 % HDPE and LDPE at 20C° show some effect after 7 days. Both at 50C° show immediate damage and are not
recommended.
Oleic acid HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. LDPE at 20C°-50C° shows
immediate damage and is not recommended.
Oxalic acid LDPE at 20C° shows some effect after 7 days. HDPE at 20C° and both HDPE and LDPE at 50C° show little or
no damage after 30 days.
Ozone HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE and LDPE at
50C° show immediate damage and are not recommended.
Perchloric acid HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE and LDPE at 50C° show immediate damage and are not recommended.
Perchloric ethylene HDPE and LDPE at 20C°-50C° show immediate damage and are not recommended.
Phenol HDPE and LDPE at 20C°-50C° show immediate damage and are not recommended.
Phosphoric acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Phosphoric acid 85% HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
immediate damage and is not recommended.
Phosphorous trichloride HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° has no
data available. HDPE at 50C° shows some effect after 7 days.
Potassium acetate No data is available at this time.
Potassium bromide No data is available at this time.
Potassium carbonate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium hydroxide 5 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium hydroxide
concentrated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium permanganate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Propylene glycol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Pyridine Immediate damage may occur. Not recommended for continuous use.
Salicylic acid, saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Silver acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Silver nitrate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium carbonate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium chloride,
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium dichromate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium hydroxide 1% LDPE at 20C°-50C° shows little or no damage after 30 days of constant exposure. HDPE at 20C°-50C° shows
some effect after 7 days.
Sodium hydroxide 50% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium hypochlorite 15% HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. LDPE at 20C° is suitable but
at 50C° shows some effect after 7 days.
Sodium nitrate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium sulphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sucrose LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulphide No additional information is available at this time.
Sulfuric acid 6% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 20% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 60% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 98% LDPE at 20C°-50C° shows little or no damage after 30 days of constant exposure. HDPE at 20C° shoes effect
after 7 days and is not recommended for use at 50C°.
Tannic acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Tetrahydrofuran HDPE and LDPE at 20C° show some effect after 7 day of constant exposure.HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Toluene LDPE at 20C° show some effect after 7 day of constant exposure. HDPE at 20C°-50C° and LDPE at 50C°
show immediate damage and are not recommended.
Trichloracetic acid HDPE and LDPE at 20C° show some effect after 7 day of constant exposure.HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Trichlorethane Immediate damage may occur. Not recommended for continuous use.
Turpentine oil HDPE and LDPE at 20C° show some effect after 7 day of constant exposure. HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Urea LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Xylene HDPE at 20C° shows some effect after 7 day of constant exposure. LDPE at 20-50C° and HDPE at 50C° show
immediate damage and are not recommended.
Zinc chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.